Broken weld, repair date in image.
Weld circled arrow on "bead" obvious recent grind, work dated as per rail procedureโฆ
CKT!
Rushed weld job, no heat treating of the rail.
304L deposition steel gives a standard, martensite-free microstructure. Heat treating the repaired rail increases hardness and eliminates the micropores. Preheating may mitigate the developed microcracks at the rail-deposition interface.